博文

目前显示的是 九月, 2021的博文

Preventive Measures Of High-Speed Warping Broken Ends

  Preventive Measures Of High-Speed Warping Broken Ends September 10,2021 I  Events   When our company produces  ST-ERL-808  products, the quality indicators such as evenness and strength have reached the user's requirements, but the warping breakage exceeds the standard in the preparation process. The user requires that the number of broken ends in warping for one million wires should be less than 0.6, but the number of broken ends in our company's warping is more than 1.8, which greatly exceeds the standard, which strictly affects the production efficiency of the subsequent process.   The ST-ERL-808 product contains 30% long-staple cotton, the fine-staple cotton grade is 2.5, and the long-staple cotton is 137 Xinjiang cotton. The two components are produced separately and are mixed in the combing preparation process to maintain a certain mixing ratio. . The specific yarn indicators are as follows: even CV 12.3%, 4 kilometers of details, 20 kilometers of thick knots, 60 kilome

Preventive Measures Of High-Speed Warping Broken Ends

  Preventive Measures Of High-Speed Warping Broken Ends September 10,2021 I  Events   When our company produces  ST-ERL-808  products, the quality indicators such as evenness and strength have reached the user's requirements, but the warping breakage exceeds the standard in the preparation process. The user requires that the number of broken ends in warping for one million wires should be less than 0.6, but the number of broken ends in our company's warping is more than 1.8, which greatly exceeds the standard, which strictly affects the production efficiency of the subsequent process.   The ST-ERL-808 product contains 30% long-staple cotton, the fine-staple cotton grade is 2.5, and the long-staple cotton is 137 Xinjiang cotton. The two components are produced separately and are mixed in the combing preparation process to maintain a certain mixing ratio. . The specific yarn indicators are as follows: even CV 12.3%, 4 kilometers of details, 20 kilometers of thick knots, 60 kilome

Characteristics of shuttleless loom

  Characteristics of shuttleless loom    Characteristics of shuttleless loom   The four  shuttleless looms  have one basic feature in common, that is, separating the filling yarn from the shuttle, or using a small and light picker instead of a large and heavy shuttle to carry several weft yarns, thus creating an advantage.    High speed filling insertion.    When filling the weft, the package is directly put on, and the weft insertion mechanism is entered through the weft storage device, so that the  loom  can get rid of frequent filling.    Therefore, the use of shuttleless loom plays an important role in increasing varieties, adjusting fabric structure, reducing fabric defects, improving fabric quality, reducing noise and improving working conditions.    Shuttleless loom has 4 ~ 8 times high speed shuttle loom;    Therefore, the large-scale popularization of shuttleless loom will greatly improve production efficiency.       Due to the improvement of shuttleless loom structure, it sel

How to avoid rapier head and belt wear on rapier loom?

图片
  How to avoid rapier head and belt wear on rapi er loom?      Rapier looms  are shuttleless looms. It is a general loom for weaving medium and small batch colored fabrics and frequently changing varieties. In the production process, the consumption of rapier loom high-speed filling insertion, rapier head and sword belt accounts for more than half of the total consumables of rapier loom. Therefore, how to effectively avoid the wear of the rapier head and sword belt is very important to save the production cost. 1. The harm of wear and tear.   At 400 revolutions per minute and 20 hours per day, the rapier head moves 960, 000 times per day. The most vulnerable parts of the head to wear are the head, wings and bottom. The head of the sword will be subjected to the friction of warp, guide hook, sword plate and guide rail every time when entering the weft. When the two wings of the jian head are badly worn and form a blade shape, it is easy to break the warp yarn, and even make the jian hea